When a printed part has to hold something, like a bracket, a hook or a clip, the instinct is to crank infill to 100%. It's rarely the most effective move. What changes strength most is how you place the part and how many walls it has. Here are the factors in order, with what Prusa and a scientific review of dozens of studies say.

1. Orientation: the layers are the weak point

A 3D printed part isn't equally strong in every direction. A review published in the journal Polymers (Syrlybayev and colleagues, 2021) singles out this anisotropic behaviour as one of the big problems of filament printing and attributes it to poor bonding between layers. It explains it with a study it cites: a line of plastic aligned with the load carries that load itself, while one running across it only has its bond with the neighbouring lines to rely on.

Prusa sums it up for PLA: on impact it tends to break along the layers or into shards, and its layer adhesion is weaker than other materials'.

Cream-coloured 3D printed part with several cracks following the layer lines
A printed housing with delamination cracks, as its author describes it: the layers have separated. · Photo: syvwlch, via Wikimedia Commons, CC BY 2.0

The practical consequence: before printing, think about which way the load will pull and place the part so that force runs along the lines of plastic instead of trying to pull the layers apart. The classic example is a hook:

The same hook printed standing, with layers crossing the load path and a crack between layers, and lying flat, with the lines following the hook's shape Standing load the load pulls layers apart Lying flat load the lines follow the shape
Simplified diagram (not a photo): the same hook printed standing and lying flat. The stripes show how the layers or extrusion lines end up.

The review also notes that, for tensile strength, most studies find better results with the part lying flat or slightly tilted (0° or 15°), although for bending and impact the results vary from study to study. If orienting it well means you need supports, tree vs normal supports covers how to add and remove them.

2. Walls before infill

Prusa is clear: going above 40% infill rarely makes sense, and its tests put the sweet spot at 10-20%. Above 20% the part gains toughness, but the same effect can be achieved by adding perimeters (walls), and its infill guide stresses that increasing the number of perimeters works better.

In practice, for a functional part, start by adding walls before touching the infill. There's more on patterns and percentages in infill: which pattern and percentage.

3. Material (and its temperature)

4. Layer height and nozzle

The Polymers review finds layer height to be the most influential of the parameters it studies, and notes that improving bonding between layers means reducing it, at the cost of slower printing. The nozzle matters too: in Prusa's tests, parts printed with a 0.6 mm nozzle absorbed up to 25.6% more energy than those from a 0.4 mm one, and they print faster (see how to print faster).

Summary: where to start

SettingWhat to do
OrientationMake the load run along the lines of plastic, not pull layers apart.
WallsAdd perimeters before infill.
Infill10-20% is usually enough; above 40% it rarely pays off.
MaterialPETG if the part takes knocks; PLA only for rigid parts without impacts.
Temperature and fanWith PETG, more temperature and less fan improve layer bonding.
NozzleA 0.6 mm one gives tougher parts if you don't need fine detail.

Frequently asked questions

Does more infill make a part stronger?
Up to a point. Prusa explains that going above 40% rarely makes sense and that its sweet spot is 10-20%. Above 20% the part gains toughness, but you get the same effect, and a better one, by adding perimeters.
Why do printed parts break along the layers?
Because the bond between layers is the weak point. A review published in Polymers attributes the anisotropic behaviour of printed parts to poor bonding between layers: a line of plastic aligned with the load carries it itself, while one running across it only has its bond with the next to rely on.
How should I orient a part to make it stronger?
Think about which way the load will pull and place the part so that force runs along the lines of plastic instead of pulling layers apart. A hook, for example, is best printed lying flat so the lines follow its shape.
Which is stronger, PLA or PETG?
It depends on what you mean by strong. According to Prusa, PLA breaks along the layers or into shards on impact, while PETG is tougher and more flexible, so it usually handles knocks and mechanical parts better.

Sources