How to print PETG: temperatures, bed, stringing and supports

PETG is the natural next step after PLA: tougher, more heat- and moisture-resistant, and still easy to print. But it has three habits that drive beginners mad: it sticks too hard to the bed, it strings, and its supports refuse to come off. Here's how to fix each one, based on what Prusa and Flashforge recommend.

What PETG is and what it's for

PETG is PET (the plastic in drinks bottles) modified with glycol so it prints better. Prusa sums it up in its material guide: easy to print, good layer adhesion, tough and durable, heat- and moisture-resistant. It's the material for mechanical parts, indoors and outdoors. If you're weighing it against others, see the comparison in PLA vs PETG vs ABS.

White functional part printed in PETG: a shaft with five pulleys
A functional part printed in PETG: exactly where this material shines. · Photo: newman72, via Wikimedia Commons, CC BY 2.0

Starting temperatures

For its PETG, Prusa recommends 230 °C for the first layer and 240 °C for the rest, with the bed at 85 °C then 90 °C. Other brands give slightly different ranges: always start from your filament's datasheet and adjust from there.

The bed: don't let it stick too hard

It surprises almost everyone: PETG bonds so strongly to a smooth PEI sheet that removing the part can tear off some of the surface. Prusa recommends printing it on a textured or satin sheet and, if you use the smooth one, applying a layer of glue stick first as a separator.

On the other side is warping. Flashforge explains that PETG shrinks more than PLA and so is more prone to lifting at the corners. Its fixes: glue on the bed, a brim, and no fan for the first 1-3 layers. If your part comes loose, the other causes are in why your print won't stick.

Stringing: dry it first

PETG tends to string (Prusa lists it among its drawbacks). Flashforge points to the main cause: moisture, because PETG absorbs it far more easily than PLA. The order of attack:

  1. Dry it. Flashforge gives 60-65 °C for 8 hours in an oven or dryer; the full table by material is in how to dry filament.
  2. Raise retraction a bit (length and speed) if strings persist after drying.
  3. Lower the nozzle temperature slightly, which Prusa says also tames them.

More causes and fixes in how to fix stringing.

New PETG filament spool in its vacuum bag inside the box
A freshly opened PETG spool, still in its vacuum bag: that's how it arrives dry, and how it should be stored. · Photo: Suit, via Wikimedia Commons, CC BY-SA 4.0

Cooling fan: depends on what you want

Prusa explains that PETG should be cooled so the part keeps its shape and to reduce stringing and oozing. But if you're after maximum strength, it suggests turning the fan off: with more heat, layers fuse better.

Supports that won't come off

The strong layer adhesion that makes PETG tough also welds supports to the part. Flashforge suggests this order:

  1. Dry the filament well: moisture makes the support stick to the underside of the part.
  2. Increase the top Z distance between support and part: it recommends 0.2-0.3 mm.
  3. Slightly lower flow or line width, recalibrating if needed.
  4. Use slim tree supports or a rectilinear interface pattern, which adhere less.

We cover it in more detail in supports: normal vs tree, and how to remove them.

Stronger parts

Prusa stresses that for a more solid part it's better to add perimeters than to raise infill. Flashforge agrees and suggests 3-6 walls, 20-50% infill and the gyroid pattern, without overdoing it, since an overly dense part warps more. We cover it in infill: which pattern and percentage to use.

Transparent PETG

To get light through a transparent PETG part, Flashforge recommends drying the filament, printing slowly (around 30 mm/s), thin 0.1 mm layers with slightly wider lines, a single wall and 100% aligned infill, more temperature and the fan off. Even so, transparency drops as thickness grows.

Carbon-fibre PETG

PETG-CF carries carbon-fibre particles that wear brass nozzles and clog small ones. Flashforge restricts it to hardened-steel nozzles of 0.4 mm or larger; if you're not sure which nozzle your printer has, see what is a hotend.

Frequently asked questions

What temperature do you print PETG at?
For its PETG, Prusa recommends 230 °C for the first layer and 240 °C for the rest, with the bed at 85 °C then 90 °C. Each brand gives its range on the filament datasheet: use that as the starting point.
Why does PETG string so much?
According to Flashforge, the main cause is moisture: PETG absorbs it more easily than PLA. Dry it first; if strings remain, raise retraction a bit. Prusa adds that slightly lowering the nozzle temperature also helps.
Why does PETG rip chunks off the bed?
Because it bonds very strongly to smooth PEI sheets, enough to damage them. Prusa recommends textured or satin sheets, or glue stick on the smooth one as a separator.
Is PETG food safe?
The material itself may be considered food safe, but a printed part is made of layers where bacteria can grow over time, as Prusa points out. If it will touch food, apply a food-safe epoxy coating.